Hello,
We have a bath to anodize the titanium that called anodizing bath. It contains sulphuric acid + de-ionized water. And there is a coming acrcreditation about chemical coating. When i check the checklist of accreditation, there is a question about titanium amount of sulphuric acid bath. ıt should be below 20 g/l. Do you guys know is there any method to determine titanium and NaCl in sulphuric acid bath.
Thanks for your help guys.
We have a bath to anodize the titanium that called anodizing bath. It contains sulphuric acid + de-ionized water. And there is a coming acrcreditation about chemical coating. When i check the checklist of accreditation, there is a question about titanium amount of sulphuric acid bath. ıt should be below 20 g/l. Do you guys know is there any method to determine titanium and NaCl in sulphuric acid bath.