Hi,
I would like to know how we can choose the best type of groundbed for the design of cathodic protection system for buried pipeline ( conventional, distributed or deep groundbed).
Thanks
 
Replies continue below

Recommended for you

Other than length of pipe, cost will be your first indicator. It wouldn't make a lot of sense to use a deep anode bed, if your pipeline was only 200m long.
 