Hi there,
I have a supplier of a component with 4" WN ANSI B16.5 600# RJ flanges. In order to reduce the overall lenght of the component, they reduce the lenght through the hub from stated 4 inch to 3.15 inch, thus saving a total of 1.7 inch on the lenght. The machine new welding ends, seems to be in line with the standard. But what about the lenght? Is it okay to reduce it without any notes or 'special considerations'?
Regards
I have a supplier of a component with 4" WN ANSI B16.5 600# RJ flanges. In order to reduce the overall lenght of the component, they reduce the lenght through the hub from stated 4 inch to 3.15 inch, thus saving a total of 1.7 inch on the lenght. The machine new welding ends, seems to be in line with the standard. But what about the lenght? Is it okay to reduce it without any notes or 'special considerations'?
Regards