What year did ansi B16.9 change the A dimension for a 3/4"
long radius 90 ell, it was 1.125" face to center now the
2003 edition call out 38mm which is about1.5 inches
Thanks
VKP1
 
Replies continue below

Recommended for you

Thanks DSB123,
Yes I did mean Asme instead of Ansi.
Do you know where I can get a copy of that year showing that
dimension 1 1/8"
 
VKP1,
I beleive the 38mm in 2003 edition is a typo.All of the tables I have call the dimension as 1.125" (28mm).
 
GENERAL NOTE: All dimensions are in millimeters.
NOTE:
(1) Ä and B dimensions of 29 mm and 11 mm, respectively,
may be furnished for NPS 9 4 (DN20) atthe manufacturer's
option.
 