canadiancastor
Structural
- Apr 13, 2014
- 38
The last time I had a look was about 10 years ago, external FRP reinforcement was next to useless because of the fire requirements in buildings (from memory, for flexure some percentage of service level loads needed to be maintained while ignoring the FRP reinforcement, which did not allow for substantial gains in resistance). Does anyone have some examples or where this can work? Any tips about how to address issues with quality control on site? I hear that it might be used for seismic retrofits in California area?