APIpipeWholesaler
Materials
- Jul 26, 2012
- 24
API 5L X52 PSL 2 30" O.D. X .875 wall
Permissable Mn is 1.65% MAX page 30 Table 5 (b)
MTR has Ladle and product Analysis
Ladle Mn 1.66
Product 1 1.60
product 2 1.60
Customer is rejecting due to the fact that the reported Ladle analysis is Mn 1.66%.
API clearly states in the very top of API Table 5 " Mass Fraction, Based on Heat and Product Analyses " Yet MTR does not specifically give a heat analyis.
API says nothing in regards to ladle analysis.
Just want to be certain that when it comes to API 5L that Product analysis overrides ladle?
As always thanx for everyone's input up front!
-=Fred=-
Vass Pipe
Vass Pipe API Line Pipe Industry Leader "
Just want to be certain that when it comes to API 5L that Product analysis overrides ladle?
As always thanx for everyone's input up front!
-=Fred=-
Vass Pipe
Vass Pipe API Line Pipe Industry Leader
Vass Pipe API Line Pipe Industry Leader
Permissable Mn is 1.65% MAX page 30 Table 5 (b)
MTR has Ladle and product Analysis
Ladle Mn 1.66
Product 1 1.60
product 2 1.60
Customer is rejecting due to the fact that the reported Ladle analysis is Mn 1.66%.
API clearly states in the very top of API Table 5 " Mass Fraction, Based on Heat and Product Analyses " Yet MTR does not specifically give a heat analyis.
API says nothing in regards to ladle analysis.
Just want to be certain that when it comes to API 5L that Product analysis overrides ladle?
As always thanx for everyone's input up front!
-=Fred=-
Vass Pipe
Vass Pipe API Line Pipe Industry Leader "
Just want to be certain that when it comes to API 5L that Product analysis overrides ladle?
As always thanx for everyone's input up front!
-=Fred=-
Vass Pipe
Vass Pipe API Line Pipe Industry Leader
Vass Pipe API Line Pipe Industry Leader