Refer to NACE MR0175-2003 Table D-2, material API 5L Grade A & B, Grade X-42 through X-65 have been accepted for sour service
But I don't find the limitation value of H2S partial pressure in both of API Spec 5L and NACE MR0175.

Can anyone explain this limitation?
 
Replies continue below

Recommended for you




for gasoil services, above .01 Mol % of H2S and at temperatures above 396ºC you begin to have higher and higher corrosion rates for the carbon steels