API 5L SPEC ... P-NUMBERS AND GROUP NUMBERS

Status
Not open for further replies.

camersa

Mechanical
May 24, 2008
2
thread292-115971
In asme BPVC section IX you found, NONMANDATORY APPENDIX D "P‐NUMBER LISTING", define de P-numbers and Group Number for Materials API 5L SPEC ...for example API 5L X52 GRADES IS P-1 AND G-1...
I have doubts if you should have impact test for the WPS specification..
 