Apr 11, 2025 #1 C Cmorse1 Mechanical Apr 11, 2025 2 Can any one explain this to me. Building a tank with a shell thickness of 3/8" and Anchor Chairs are 1/2". Does code csall for PT Final
Can any one explain this to me. Building a tank with a shell thickness of 3/8" and Anchor Chairs are 1/2". Does code csall for PT Final
Saturday at 5:04 AM #2 IRstuff Aerospace Jun 3, 2002 44,735 This is the wrong forum for this question. Please delete your post and post in the correct one.
Monday at 1:46 PM #3 JStephen Mechanical Aug 25, 2004 8,695 I would interpret that wording to mean each part has to be greater than 3/4", not that the sum of the thicknesses is greater than 3/4", so I would say "no". That could be reworded more clearly.