I got an issue regarding the construction of API 650 tank with 60 mm thickness shell plates and 15C design metal temperature.
the inspector ask to perform the PQR for SMAW welding process with impact tests , im my opnion there is no reson to perform impact test becuse of the design metal temperature.
please advise.
THX,
I got an issue regarding the construction of API 650 tank with 60 mm thickness shell plates and 15C design metal temperature.
the inspector ask to perform the PQR for SMAW welding process with impact tests , im my opnion there is no reson to perform impact test becuse of the design metal temperature.
please advise.
THX,