We have a 47 ft dia , CS tank with IFR and an Aluminum Dome Roof, Can this tank be classified as an open roof tank for top angle size determination?
As per our understanding for top angle clause 5.9.3.2 applies and we specified TOP angle as 75x75x6 mm where as client insists on using 75x75x10 mm as per clause 5.1.5.9 e
Also if client specifications call for CA for Shell, does it apply to TOP angle as well
Regards,
Aamir