Mar 12, 2003 #1 UliR Mechanical Mar 12, 2003 11 GB Hello everybody, I would like to know the minimum thickness of the bottom plate of an athmospheric storage tank. What does API 650 say? Thanks for any reply UliR
Hello everybody, I would like to know the minimum thickness of the bottom plate of an athmospheric storage tank. What does API 650 say? Thanks for any reply UliR
Mar 12, 2003 #2 IFRs Petroleum Nov 22, 2002 4,633 US API 650 minimum bottom plate thickness is 1/4" [6mm] exclusive of any corrosion allowance, and 72" [1800mm] in width. Upvote 0 Downvote
API 650 minimum bottom plate thickness is 1/4" [6mm] exclusive of any corrosion allowance, and 72" [1800mm] in width.
Mar 12, 2003 Thread starter #3 UliR Mechanical Mar 12, 2003 11 GB Hello IFRs, thanks for your fast and helpfull reply. Greetings from Cologne in Germany UliR Upvote 0 Downvote