Hello everybody,

I would like to know the minimum thickness of the bottom plate of an athmospheric storage tank. What does API 650 say?

Thanks for any reply

UliR
 
Replies continue below

Recommended for you

API 650 minimum bottom plate thickness is 1/4" [6mm] exclusive of any corrosion allowance, and 72" [1800mm] in width.
 