Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API 650 Two-Side Welding

Status
Not open for further replies.

JXWu

Petroleum
Oct 26, 2015
24
Dear experts,
Is it a API 650 requirement that the second side of a double-side welded joint needs to be back-chipped at least one-third of the joint thickness?
I cannot find this requirement in the API 650 12th edition. Need advice.
Thanks
 
Replies continue below

Recommended for you

Dear JXWu,

Are you constructing a double-walled dome roofed tank?

Regards.

DHURJATI SEN
Kolkata, India

 
This is a API 650 single wall cone roof tank
 
Status