Please tell me what topics should i prepare of API 650 Chapter # 5. Body of knowledge is confusing me about chapter # 5.
 
Replies continue below

Recommended for you

Dear blaqesmith,

You need to see under the followings for API 650 Section 5

WELD SIZES FOR SHELL & ROOF OPENINGS
Familiar with determining the sizes and spacing of welds for shell openings to the
extent of being able to use the information in the following Figures and Tables

a) API-650, Figures 5-7A, 5-7B, 5-8, 5-9, 5-12, 5-14, 5-16, 5-17, 5-19, 5-20, 5-21
b) API-650, Tables 5-6, 5-7, 5-9

Steven Loo
 