API STD 1104 - Paragraph 6.2 - Thickness

Status
Not open for further replies.

Jeldon

Chemical
May 20, 2013
25
What qualified thickness range for a welder, described by the standard API STD 1104, using a test coupon with 9.5 mm wall thickness, combination processes where the thickness of the deposit was 3.0 mm in GTAW process, and 6.5 mm in the SMAW process.
 
Replies continue below

Recommended for you

Jeldon,
This is my interpretation as combination of processes is not as clearly spelt out in API 1104 as it is in ASME IX.
9.5 mm WT gives you a qualification range of 4.8 mm to 19.1 mm as per 6.2.2 (e).
Unlike ASME you cannot use the processes separately unless you have performed two separate qualification tests as per 6.2.2 (a)

2. A change in the combination of welding processes,
unless the welder has qualified on separate qualification
tests, using each of the welding processes that are to be
used for the combination of welding processes.

Regards,
DD
 
DD,

Thanks for your answer. My understanding is the same as yours.

Best regards,
Jeldon
 