Hi,

Is supplementary requirement S12 of SA-788 applicable to hubbed tubesheet in SA-182 F316?
This is applicable for example to SA-765 forgings (explicitly recalled in SA-788), but I would like to understand if this is technically needed also for SA-182 F316 forging.