TMcRally
Automotive
- Aug 17, 2007
- 149
I'm having trouble finding information on shear loads for clinch studs.
In particular these are SS400 material studs - M4 X 12 pressed into 3mm 304SS sheet to attach 2mm Zinc plated black mild steel brackets that will be subject to impact loads. I note they have reduced torque settings over bolted joints so I am worried about using them.
In particular these are SS400 material studs - M4 X 12 pressed into 3mm 304SS sheet to attach 2mm Zinc plated black mild steel brackets that will be subject to impact loads. I note they have reduced torque settings over bolted joints so I am worried about using them.