I am working on various designs and construction methods
for an artifical reef in the Uk to create surf for recreation and also provide some shore protection. The reef requires specific slope profiles.
We have various options from a sand filled bag core covered
with concrete fabric mattress to an all concrete reef of Prepakt concrete (basically rock filled with pressurised
concrete to fill the spaces} Probably too expensive.
Sand filled bags alone have been used in various locations with partial success they move and get damaged.
I would like comments from anyone who has tried this type work and anyone who has used stonger material than nylon
in marine applications as we might make large samd filled bags out of a really strong fabric .
Dave Ritchie
Intrusion Prepakt Canada
for an artifical reef in the Uk to create surf for recreation and also provide some shore protection. The reef requires specific slope profiles.
We have various options from a sand filled bag core covered
with concrete fabric mattress to an all concrete reef of Prepakt concrete (basically rock filled with pressurised
concrete to fill the spaces} Probably too expensive.
Sand filled bags alone have been used in various locations with partial success they move and get damaged.
I would like comments from anyone who has tried this type work and anyone who has used stonger material than nylon
in marine applications as we might make large samd filled bags out of a really strong fabric .
Dave Ritchie
Intrusion Prepakt Canada