Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME Allowable Stress Values for Low Temperatures 4

Status
Not open for further replies.

Mark1arm

Mechanical
Sep 30, 2014
11
Does anyone know how to determine allowable stress values for low temperatures. I need to know what ASME states for design temperature if I am designing a vessel for operation at -196°C. For example: I am using SA240 304. the allowable stress (ATM) = 206.9 MPa, Allowable stress (DT ((@-196°C)) = ???
 
Replies continue below

Recommended for you

It is the same design stress.

At that temperature however, additional impact testing requirements will need to be addressed due to low temperature embrittlement.

Cheers,
 
The allowable stress for SA-240 304 at atmospheric temperature is 138 MPa not 206.9 MPa. There are increased low temperature allowables in table ULT-23.
 
Sorry should have mentioned I am referring to 1998 Ed. for CFR stress requirements.

Thanks for everyone's input on this!!
 
@Mark1arm,
I believe your question is addressed in General Note (e) for table 1A in II-D.

"(e) Stress values for -20°F to 100°F are applicable for colder temperatures when the toughness requirements of Section III,VIII, or XII are met."
 
Status