I have purchased some big stainless steel reducers designed according to ASME B16.9.

In order to qualify the desing, I have asked to the manufacturer the proof testing, but I got a certificate relevant to a carbon steel reducer.

So my question is: can a proof test certificate relevant to a carbon steel fitting be used to qualify a stainless steel fitting?
What is the correct interpretation of Para 9.3.4 about steel grade?

Thank you in advance to everybody.

Regards

Metma
 
Replies continue below

Recommended for you

You mean paragraph 9.4.3.

Interesting question. I would tend to think it's fine, but I can imagine some situations where it might not be. Maybe you should request an interpretation from ASME.
 
Thank you for your reply, I confirm that the correct paragraph is 9.4.3.

I have already asked and interpretation to ASME, and they reply to me that they will take care of the question during next commitee meeting (next month).

Once I will have the reply, I will post it.

Regards