Table 323.2.2 A-3 (b)

Weld Metal Deposits, What it means ?

Do I need to impact test only weld metal deposits? or HAZ too?

 
Replies continue below

Recommended for you

Deposited weld metal and the HAZ are required to be impact tested. Refer to Note 2.

 