gitsunil
Mechanical
- Aug 11, 2003
- 7
Dear Members,
I need your help with regard to CODE stamping. We have a LOOP REACTOR (datasheet attached) in one of the PP plant (in INDIA) which needs to be Code stamped.
As highlighted in YELLOW in sheet 3 of the datasheet, bottom spool pieces are having SITE WELDS (to facilitate the alignment with the PUMP at site).
LOOP REACTOR vendor is stating that since SITE WELD is involved, final hydro testing and CODE STAMPING needs to be done AT SITE and to avoid this he has proposed following (vendor email embeded):
QUOTE
Dear Sir,
with reference to section 7.0 of PIM minute, I would share with you the following consideration about final hydrotest and equipment certification of Loop Reactors RR-2001/2002.
The only weld and tests activities at site involve the lower spools connect with pump, for which loose flanges with blind are supplied.
Based on that, we are going to complete whole reactor leg fabrication, test and certification prior delivery. However, since the lower spools are currently part of ASME certified equipment, the whole equipment final hydrotest and certification can not be performed until the last loose flanges will be welded to the spool at site. This would require whole equipment hydrotest at site, with VENDOR and Authorized inspector presence at site, with significant cost and schedule impact.
Instead, we propose to segregate the spool certification from the Reactor ASME certification: the Reactor (without lower spools connected with pump) will be hydrotested and then certified with ASME nameplate by Authorized Inspector, before delivery. Spools will be certified by us as piping component according to ASME B31.3, without ASME stamp/nameplate, and then completed and tested at site by TECNIMONT, with VENDOR supervision if any (to be agreed). In this case the involvement of ASME authorized inspector at site is not required.
The above proposal, already shared with our Authorized Inspector, would require a "formal" revision of documentation (drawing, calculation, ITP, serial number) to segregate spool certification and MDR from reactor certification and MDR.
Please review the above and provide your feedback,
thank you
Best Regards
LOOP REACTOR VENDOR
UNQUOTE
What is your opinion about Vendor’s proposal?
Can we certify the bottom SPOOLS as PIPING components? If yes, HOW? Is it permitted?
How to qualify this? By which code/ method? Reference?
I would highly appreciate your swift reply.
Many thanks for your usual help,
Best regards,
Sunil Agrawal
I need your help with regard to CODE stamping. We have a LOOP REACTOR (datasheet attached) in one of the PP plant (in INDIA) which needs to be Code stamped.
As highlighted in YELLOW in sheet 3 of the datasheet, bottom spool pieces are having SITE WELDS (to facilitate the alignment with the PUMP at site).
LOOP REACTOR vendor is stating that since SITE WELD is involved, final hydro testing and CODE STAMPING needs to be done AT SITE and to avoid this he has proposed following (vendor email embeded):
QUOTE
Dear Sir,
with reference to section 7.0 of PIM minute, I would share with you the following consideration about final hydrotest and equipment certification of Loop Reactors RR-2001/2002.
The only weld and tests activities at site involve the lower spools connect with pump, for which loose flanges with blind are supplied.
Based on that, we are going to complete whole reactor leg fabrication, test and certification prior delivery. However, since the lower spools are currently part of ASME certified equipment, the whole equipment final hydrotest and certification can not be performed until the last loose flanges will be welded to the spool at site. This would require whole equipment hydrotest at site, with VENDOR and Authorized inspector presence at site, with significant cost and schedule impact.
Instead, we propose to segregate the spool certification from the Reactor ASME certification: the Reactor (without lower spools connected with pump) will be hydrotested and then certified with ASME nameplate by Authorized Inspector, before delivery. Spools will be certified by us as piping component according to ASME B31.3, without ASME stamp/nameplate, and then completed and tested at site by TECNIMONT, with VENDOR supervision if any (to be agreed). In this case the involvement of ASME authorized inspector at site is not required.
The above proposal, already shared with our Authorized Inspector, would require a "formal" revision of documentation (drawing, calculation, ITP, serial number) to segregate spool certification and MDR from reactor certification and MDR.
Please review the above and provide your feedback,
thank you
Best Regards
LOOP REACTOR VENDOR
UNQUOTE
What is your opinion about Vendor’s proposal?
Can we certify the bottom SPOOLS as PIPING components? If yes, HOW? Is it permitted?
How to qualify this? By which code/ method? Reference?
I would highly appreciate your swift reply.
Many thanks for your usual help,
Best regards,