ASME - Flat Unstayed head- Joint Efficiency

Status
Not open for further replies.

skumark

Mechanical
Sep 17, 2009
2
UG-34-Can I use E=1, if the flat head is seamless? Or does E have to be the joint efficiency of weld connecting flat head to shell? Please help!
 
Replies continue below

Recommended for you

The category A of weld, even if it is within the flat head (refer UW-3(a)), it can be E=1 for type 1 of welds per table UW-12. The weld of the flat head to the shell is a C category weld per UW-3(c).
Cheers,
gr2vessels
 
Many Thanks gr2. Therefore I presume E=1 is correct for a seamless head.
 