WE91
Industrial
- Nov 29, 2023
- 13
When performing Impact testing in multiprocess PQRs in accordance with B31.3 or Section VIII does the root pass process require impact testing when deposited thickness excluding reinforcement is less than 2.5mm? Both codes have impact exemptions for material less than 2.5mm but would the root pass fall under this exemption? Example PQR is 1" thick GMAW/FCAW and impacts are performed to -320F,the root pass was GMAW with FCAW hot pass, fill, and Cap. GMAW excluding reinforcement deposited is only 1/16"(.0625"/1.58mm) is my GMAW/FCAW WPS compliant with -320 impacts?
Thanks in advance!