I have a PQR with base metal P1Gr2 to P1Gr2 without impact testing (specifically, SA-516 GR.70 welded to itself).

The corresponding WPS is for base metals P1Gr1,2&3 to P1Gr1,2&3.

I believe the additions of groups 1 and 3 on the WPS are a result of QW-403.5

Is this corrrect? Please Advise. Thank You.
 
Correct. The Group numbers come into play for WPS qualification under impact test requirements.
 
When you ask if the group numbers on this WPS are being added as a result of QW403.5, I would say not, because, QW403.5 is a supplementary variable and as such is not applicable for a non-impact qualified WPS.
To clarify further, on a WPS, the Group Numbers only come into play when impact testing is required. Your WPS could simply provide the P number, in this case P1, without specifically listing any group numbers. There's nothing wrong with listing group numbers, but, in this case it isn't required per QW403.5.
 
weldtek;
I probably should have better explained my correct statement. I focused on the entire wording of the note. In this case, from a broad perspective the second paragraph implies to me that for ferrous materials when a P-No is qualified to itself and other P-No, the Group numbers come along with it. The third paragraph in this note states when impact testing is required this does not apply.
 
Thank you for the timely responses. What i have gathered from your posts is that since impact testing was not required, Group No. becomes a non-essential variable and can therefore be changed without the need for requalification.

So it would follow that my WPS isn't necessarily 'wrong' for listing Group No. 1,2&3 but this WPS would still not allow me to weld any P1Gr4 metals, and therefore a more 'accurate' WPS would display something along the lines of "All", "N/A" or simply leave the space blank altogether.
 