Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME SA-212-Grade B FBX quality

Status
Not open for further replies.

POPPASMURFF1942

Petroleum
Joined
Nov 2, 2006
Messages
11
Location
US
Performing fitness for service calculations on a 1950 vintage vessel. I need Max allowable stress as well as yield . Vessel operates at 250 degrees. In the day MDMT was not thought of so what would be the most like material today to calculate a MDMT too.
 
The SA 212 was replaced by SA 515-70 plate material(coarse grained practice) specification in 1966.

I was able to access my archive file and found the following information

SA 212 B

UTS 70-85 Ksi
min YS 38 Ksi

In one of the reputable data resources, the minimum design metal temperature for this material can be as high as 120 deg F. This is the reason this material was used in Section I boilers where operating temperatures were well above ambient to ensure adequate notch toughness behavior.
 