AK23Static
Mechanical
- Oct 21, 2012
- 11
We have Pig trap (ASME Sec VIII Div1) under Lethal Service having Quick opening door (QOC).
Vessel requires PWHT per UW-2 Lethal service requirements.
Query: Quick opening Closure (QOC) was welded to Pig trap and the PWHT was done inline with Code requirements for Lethal Service. However the Closure door which was hinged to QOC was removed and has not undergone PWHT.
Is this is acceptable scenario to have hinged part not undergoing PWHT and what is the specific reference in DIV1 for such [highlight #FCE94F]exemption.[/highlight]
cheers
AK
Beginning of every success is desire
Vessel requires PWHT per UW-2 Lethal service requirements.
Query: Quick opening Closure (QOC) was welded to Pig trap and the PWHT was done inline with Code requirements for Lethal Service. However the Closure door which was hinged to QOC was removed and has not undergone PWHT.
Is this is acceptable scenario to have hinged part not undergoing PWHT and what is the specific reference in DIV1 for such [highlight #FCE94F]exemption.[/highlight]
cheers
AK
Beginning of every success is desire