Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME SEC VIII UW 13(e)

Status
Not open for further replies.

david339933

Industrial
Jun 15, 2011
1,204
ASME SEC VIII UW 13(e) states "When shells, heads, or other pressure parts are welded to a forged or rolled plate to form a corner joint, as in Fig. UW-13.2......" does rolled plate mean rolled by the mill in producing the plate or does it mean flat plate rolled to a radius after manufacture?
 
Replies continue below

Recommended for you

david339933, most often the interpretation would be plate rolled at the mill, normally applied to flat heads or tubesheets, etc. attached to a cylindrical shell. Other interpretations may be applicable depending on the details of construction.

Regards,

Mike
 