Is he certified??
Per QW-304
Alternatively, welders may be qualified by volumetric NDE QW-191 when making a groove weld using SMAW, SAW, GTAW, PAW, and GMAW (except short circuiting mode for radiographic examination) or a combination of these processes.
6" SCH 40 pipe
Root pass - GMAW-S (Short circuit)
Cover pass - GMAW-P (Pulse)
The part I'm hung up on is it obviously says NO for short circuit ..BUT.. it also says OR a combinations of these processes. So does that mean you can't certify with RT if there's short circuit involved at all? Or is it allowed because it's a combination of processes.
Per QW-304
Alternatively, welders may be qualified by volumetric NDE QW-191 when making a groove weld using SMAW, SAW, GTAW, PAW, and GMAW (except short circuiting mode for radiographic examination) or a combination of these processes.
6" SCH 40 pipe
Root pass - GMAW-S (Short circuit)
Cover pass - GMAW-P (Pulse)
The part I'm hung up on is it obviously says NO for short circuit ..BUT.. it also says OR a combinations of these processes. So does that mean you can't certify with RT if there's short circuit involved at all? Or is it allowed because it's a combination of processes.