I am working on the elastic plastic analysis of ASME Section VIII Division 2 Part 5.
The material is SA-285 Gr. C, the Design Pressure is 0.3MPa at Design Temperature 200degC.
I use the ANSYS 2024 R1 for the analysis.
The material model with true stress-strain curve has been added as per Annex 3-D into the Multilinear Isotropic Hardening.
The large displacement for non-linear geometry is activated.
The load combination with design margin also been applied as per Table 5.5.
If refer to ASME PTB-3, Figure E5.2.3.2, it present the result of Von-Mises stress and Equivalent Plastic Strain.
And Figure E5.2.3.3, it is showing the Pressure vs Displacement.
Question:
What is the acceptance criteria for this analysis? Since the ASME only says "if the convergence is achieved, the component is stable under the applied loads".
How do we know if the analysis is convergence?
What would happen if the analysis is not convergence?
What is the applicable result to be showing in the report?
Shall we plot the result in the True Stress-Strain curve?
I have seen the several thread for this topic, but still didn't get the clear answer.
Thank you.
I am working on the elastic plastic analysis of ASME Section VIII Division 2 Part 5.
The material is SA-285 Gr. C, the Design Pressure is 0.3MPa at Design Temperature 200degC.
I use the ANSYS 2024 R1 for the analysis.
The material model with true stress-strain curve has been added as per Annex 3-D into the Multilinear Isotropic Hardening.
The large displacement for non-linear geometry is activated.
The load combination with design margin also been applied as per Table 5.5.
If refer to ASME PTB-3, Figure E5.2.3.2, it present the result of Von-Mises stress and Equivalent Plastic Strain.
And Figure E5.2.3.3, it is showing the Pressure vs Displacement.
Question:
What is the acceptance criteria for this analysis? Since the ASME only says "if the convergence is achieved, the component is stable under the applied loads".
How do we know if the analysis is convergence?
What would happen if the analysis is not convergence?
What is the applicable result to be showing in the report?
Shall we plot the result in the True Stress-Strain curve?
I have seen the several thread for this topic, but still didn't get the clear answer.