Hello,
I would appreciate if someone could elaborate on the following text at the bottom of table 5.7 in ASME VIII, Division 2:

"(3) E is the % elongation and RA is the % reduction in area determined from the applicable material specification."

How would one go about to obtain these parameters (E & RA)? What are typical values for an arbitrarily chosen steel?

Thank you,
 
Replies continue below

Recommended for you

The values are obtained from the individual material specification. Often only one of the two will be provided.
 