AF-402 3rd sentence states"The exemptions for post weld heat treatment in Tables AF-402.1 and 402.2 are not permitted when the vessel is designed for lethal service. (AG-01.1(c)...."
However, the Notes of Table AF-402.1 for P1 material (2)(b)1,2,3,4, list conditions where heat treatment is NOT Mandatory even if the vessl is designed for lethal service (AG 301.1 (c).
Question: Is PWHT required for welds if the conditions listed in Table AF-402 for P1 material Note (2) (b)1,2,3,4, are met ?
Proposed answer: No
Is there an interpretation on this subject ?
I would appreciate any comments.
 
Replies continue below

Recommended for you

The exemptions for post weld heat treatment in Tables AF-402.1 and 402.2 are not permitted when the vessel is designed for lethal service. (AG-01.1(c)...."

Yes, this is correct. Read Footnote 3 for what is lethal service.

However, the Notes of Table AF-402.1 for P1 material (2)(b)1,2,3,4, list conditions where heat treatment is NOT Mandatory even if the vessel is designed for lethal service (AG 301.1 (c).

No. The Table does not apply for exemptions to PWHT based on AF-402 and Footnote 3.

 