golfdesigner
Civil/Environmental
We just had a contractor finish paving, all binder went down in good weather, and about 25% of surface went down at same time as binder. The remainder of the finish surface course 1.5 inches went down in intermittant drizzle, with some ponding water on binder that he paved right over.
What kind of potential problems will there be in the short term and the long term with paving done under these conditions. The air temperature was in upper 60's at time of paving and the mix came om covered trucks from a plant about 20 minutes away.
Any and all comments welcome. Thanks
What kind of potential problems will there be in the short term and the long term with paving done under these conditions. The air temperature was in upper 60's at time of paving and the mix came om covered trucks from a plant about 20 minutes away.
Any and all comments welcome. Thanks