Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SDETERS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A 53 Gr .B ERW WELDS HEAT TREATED?

Status
Not open for further replies.

CREERAAM

Mechanical
Feb 23, 2015
109
Experts,

Hai, The following line is Mandatory in Pipes and to be mentioned in MTC's? "The weld seam of electric-resistance welded pipe in Grade B shall be heat treated after welding".

REGARDS,

G.SRIRAM.

Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action
 
Replies continue below

Recommended for you

Not sure I completely follow your question. But let's see if I'm on the right path.

Yes, according to ASTM Specification A53, it reads as follows:

4. Materials and Manufacture

4.3 The weld seam of electric-resistance welded pipe in Grade B shall be heat treated after welding to a minimum of 1000 °F [540 °C] so that no untempered martensite remains, or
otherwise processed in such a manner that no untempered martensite remains.​
 
This is commonly done by the mill using an induction heating unit. We used a TOCO unit for this purpose.
 
Status