There are companies advertising fittings as A234 - Gr 4130. It doesn't appear that any of the A234 grades listed in table 1, of the ASTM specification, have the chemical composition range to allow 4130. How are they doing this?
 
Replies continue below

Recommended for you

Which companies? Foreign? There are fittings supplied as 4130 with no reference to A 234.
 
Other than by not following the rules?
In some spec systems (SAE) people often take exceptions.
Under the rules of ASTM you cannot identify a material or product as meeting a spec unless it meets all of the requirements, no exception allowed. Occasionally you see something marked as "ex" but it is a tighter or additional requirement

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
metengr,

Yes, the companies are based in the UK. I've attached a screenshot from one of their specification pages.

EdStainless,

That is what I thought. Section 5 of the ASTM A234 specification doesn't appear to allow for variance outside of the values listed in Table 1.

Thank you both for your input.
 