APIpipeWholesaler
Materials
- Jul 26, 2012
- 24
We are supplying pipe on a fast track job that requires material from stock.
Customer has requested ASTM A252 Gr 3 with 50 KSI min yield or better.
After placing the order they are requesting that all MTR's state "M" or modified due to the 50 KSI YS.
No where in the spec is there any reference to a "Modified" inclusion reported on an MTR.
I want to just be able to tell them stock pipe will NOT carry a Modified remark and it will be up to
our and their QC team to verify each and every piece.
Has anyone ever heard of, outside of a mill order, A252 pipe carrying OR requiring a modified statement?
Thanx in advance
Vass Pipe Pipe Salesperson and Mgr.
Vass Pipe API Line Pipe Industry Leader
People do what you inspect, not expect!
Customer has requested ASTM A252 Gr 3 with 50 KSI min yield or better.
After placing the order they are requesting that all MTR's state "M" or modified due to the 50 KSI YS.
No where in the spec is there any reference to a "Modified" inclusion reported on an MTR.
I want to just be able to tell them stock pipe will NOT carry a Modified remark and it will be up to
our and their QC team to verify each and every piece.
Has anyone ever heard of, outside of a mill order, A252 pipe carrying OR requiring a modified statement?
Thanx in advance
Vass Pipe Pipe Salesperson and Mgr.
Vass Pipe API Line Pipe Industry Leader
People do what you inspect, not expect!