We have procured ASTM A333 GRADE 6 for sour service and there are two points that need clarification.
1. in the material requisition there is a requirement for yield strength and ultimate tensile strength not to exceed the specified minimum value by more than 20,000 psi. However the MTC depict higher YS and UTS than specified.
2. pipes are Quenched & Tempered, instead of Normalized as required for Sour Service.
The questions are:
1. who can the yield strength and tensile strength reach such high values, and if it affects the behavior of the pipe in the sour service.
2. is there a possibility Quenched and tempered to be accepted, for example an additional heat treatment or testing?
Thank you in advance
1. in the material requisition there is a requirement for yield strength and ultimate tensile strength not to exceed the specified minimum value by more than 20,000 psi. However the MTC depict higher YS and UTS than specified.
2. pipes are Quenched & Tempered, instead of Normalized as required for Sour Service.
The questions are:
1. who can the yield strength and tensile strength reach such high values, and if it affects the behavior of the pipe in the sour service.
2. is there a possibility Quenched and tempered to be accepted, for example an additional heat treatment or testing?
Thank you in advance