wijaya1
Petroleum
- Feb 20, 2008
- 3
Could anybody tell me the MDMT of ASTM A36 steel for designing 35 psi MAWP pneumatic tank? Based on discussion of Sam Cheung et al, I am under the impression that as per ASME COde Sec VIII, Fig UCS 66 M, the minimum temperature recommended without the need to conduct Impact test is +20 deg. F or -7 deg. C.
Someother information I received from steel supplier is not to be used below 5 deg. C.
Any shed of light on this matter is much appreciated
Someother information I received from steel supplier is not to be used below 5 deg. C.
Any shed of light on this matter is much appreciated