XL83NL
Mechanical
- Mar 3, 2011
- 3,109
Dear all,
I was looking at the ASTM B619/B622 standards (2004 version) for nickel alloy piping.
I noticed it said the sizes are acc to ASME B36.319M, meaning, sizes go to Sch 80 (for B619).
Does this mean Sch 160 and Sch XXS isnt available for e.g. Hastelloy C-276 pipe?
Or am i mislead by some misinterpretation?
Or is there some other ASTM that covers nickel alloy piping up to sch 160/XXS?
I'd like to know this since Im calculating a pipe spec, where the pipe's MAWP meets the rating of B16.5 group 3.8 2500 lbs WNRF flanges.
Thanks in advance for any help/advice.
I was looking at the ASTM B619/B622 standards (2004 version) for nickel alloy piping.
I noticed it said the sizes are acc to ASME B36.319M, meaning, sizes go to Sch 80 (for B619).
Does this mean Sch 160 and Sch XXS isnt available for e.g. Hastelloy C-276 pipe?
Or am i mislead by some misinterpretation?
Or is there some other ASTM that covers nickel alloy piping up to sch 160/XXS?
I'd like to know this since Im calculating a pipe spec, where the pipe's MAWP meets the rating of B16.5 group 3.8 2500 lbs WNRF flanges.
Thanks in advance for any help/advice.