Jun 22, 2005 #1 112275 Marine/Ocean Jan 8, 2003 58 0 0 CA Could anyone help me with locating a lab that would be able to conduct this test on a foam sample. ASTM D-2842-69
Could anyone help me with locating a lab that would be able to conduct this test on a foam sample. ASTM D-2842-69
Jun 23, 2005 #2 RichGeoffroy Materials Apr 30, 2004 64 0 0 US Try contacting Specialized Technology Resources (STR) at (860) 749-8371. Ask for Bill Tenero. Rich Geoffroy Polymer Services Group polyserv@cox.net Upvote 0 Downvote
Try contacting Specialized Technology Resources (STR) at (860) 749-8371. Ask for Bill Tenero. Rich Geoffroy Polymer Services Group polyserv@cox.net
Jun 23, 2005 Thread starter #3 112275 Marine/Ocean Jan 8, 2003 58 0 0 CA Thanks Rich I will give them a try. Upvote 0 Downvote