charlieroc
Geotechnical
- Jul 26, 2004
- 10
I am considering buying the test set for the 4253 procedure (laboratory vibratory compaction) so that I can perform field density test on 3" minus soils that have an aboundance of aggregate retained on the 3/4" sieve (say 50 to 70 percent retained 3/4" sieve). Once I find the maximum density in the lab via ASTM 4253, do I specify 90% or 95% of that number in the field when the contractor is trying to compact it under a future structure? Is 4253 equivalent to ASTM D 1557 (if I ask for 95% of 1557 should I ask for 95% of 4253?)