We manufacture large grinding and cutting equipment. Recently we produced a grinder with an automatic tool changing system but have been experiencing problems with the tools sticking in the taper. We are using a SKF 50 style taper and an OTT Jacob clamp/push cylinder for holding/ejecting the tool in the grinder.
The OTT Jacob cylinder gives about 1000kg of push to eject the tool. The tools are made from EN19 and the tapers have been surface hardened (Nitrided). There is a problem with rust forming on the surface of the tool and the female taper of the grinder, but only where the tool/grinder actually touch.
This pic shows that the thin end of the taper (in open air inside the grinder) has very little rust compared to the rest of the taper.
shows the inside of the grinder.
The equipment is working in a fully covered building (main doors always wide open), about 500km from the nearest sea.
Does any know why the rust is building up in these areas? Is it due to fretting?
Is there any lubrication we should be looking at to coat the spindle?
Anyone else have problems with tools not ejecting?
Thank you for any help you can supply.
The OTT Jacob cylinder gives about 1000kg of push to eject the tool. The tools are made from EN19 and the tapers have been surface hardened (Nitrided). There is a problem with rust forming on the surface of the tool and the female taper of the grinder, but only where the tool/grinder actually touch.
This pic shows that the thin end of the taper (in open air inside the grinder) has very little rust compared to the rest of the taper.
shows the inside of the grinder.
The equipment is working in a fully covered building (main doors always wide open), about 500km from the nearest sea.
Does any know why the rust is building up in these areas? Is it due to fretting?
Is there any lubrication we should be looking at to coat the spindle?
Anyone else have problems with tools not ejecting?
Thank you for any help you can supply.