M249Gunner
Military
Can anyone tell me where in AWS D1.1 it clarifies whether I should be bending to test "Longitudinal" face and root bends or "Transverse" (See Fig. 4.11) face and root bends for weld procedure qualification? The way it is written, it appears that I need to do both. However, any testing documents I've ever seen show only four (4) areas or spaces to record results. This implies that 2 root bends and 2 face bends (as well as the 2 tensile specimans) come from one test plate. That leads me to believe that it either comes from the "Longitudinal" bends OR the "Transverse" bends; not both.
Again, can anyone tell me where it clarifies which one to use (or both if that's the case)for procedure qualification? BTW...my base material is .187" thick, AISI steel.
Thanks,
M249Gunner
Again, can anyone tell me where it clarifies which one to use (or both if that's the case)for procedure qualification? BTW...my base material is .187" thick, AISI steel.
Thanks,
M249Gunner