Can somebody explain the following code to me?
AWS D1.1 (2008) Table 4.5 (PQR essential Variable changes requiring WPS Requalification.......) Item 33:
A Change exceeding the tolerances of 3.12, 3.13, 3.13.4, 5.22.4.1, 5.22.4.2 involving:
(1) A decrease in the groove angle
(2) A decrease in the root opening
(3) A decrease in the root face
My question:
(a) Sections 3.12, 3.13, 3.13.4 are used for prequalification. Based on Table 4.5, they are also applied to tested welding procedure qualification, right?
(b) Suppose we use single-V-grove butt joint, FCAW (B-U2-GF) in PQR. Groove angle 45 Degree, Root opening: 5mm, Root Face: 2mm. What is the qualified Groove angle; Root opening; and Root Face?
(c) How to use the above (b) condition to qualify a fillet welding? Do we need consider the joint design as a essential variable for a fillet welding?
Thanks
AWS D1.1 (2008) Table 4.5 (PQR essential Variable changes requiring WPS Requalification.......) Item 33:
A Change exceeding the tolerances of 3.12, 3.13, 3.13.4, 5.22.4.1, 5.22.4.2 involving:
(1) A decrease in the groove angle
(2) A decrease in the root opening
(3) A decrease in the root face
My question:
(a) Sections 3.12, 3.13, 3.13.4 are used for prequalification. Based on Table 4.5, they are also applied to tested welding procedure qualification, right?
(b) Suppose we use single-V-grove butt joint, FCAW (B-U2-GF) in PQR. Groove angle 45 Degree, Root opening: 5mm, Root Face: 2mm. What is the qualified Groove angle; Root opening; and Root Face?
(c) How to use the above (b) condition to qualify a fillet welding? Do we need consider the joint design as a essential variable for a fillet welding?
Thanks