CountryBoy19
Mechanical
- Jan 16, 2024
- 4
I'm being told by a Welding Engineer that in order to repair welds on a 6061 (T6) structure the entire HAZ must be removed. The structure is primarily 1/4" wall structural extrusions with 1/4 fillet welds and some bevel welds. The structure was supposed to be welded IAW AWS D1.2, cyclically loaded structures but it was not and quality control missed it. It was sent out and cracks developed in some craters that were left unfilled. To what extent does the weld need to be removed before repair welds can be made? If we remove 1/4" of parent material HAZ beyond all weld materials we won't have structure left to weld to. Is that right? I questioned the engineer on this recommendation and he said, "Yeah, you're better off starting over."
Welding engineer says at least 1/4" of parent material beyond all weld material has to be removed in order to remove entire HAZ. Note: he was not the original design engineer, just an engineer that was consulted on the repair. I personally think he is possibly being conservative or possibly misquoting standards/specs?
D1.2 doesn't specify.
Discussion on AWS forum seems to indicate 1/2" beyond all cracks or grind and verify crack is totally removed using dye penetrant or other inspection equipment and techniques.
Anybody here have thoughts? I'm likely going to run an FEA to determine the effects of the HAZ being left in place but I also want input from others.
Welding engineer says at least 1/4" of parent material beyond all weld material has to be removed in order to remove entire HAZ. Note: he was not the original design engineer, just an engineer that was consulted on the repair. I personally think he is possibly being conservative or possibly misquoting standards/specs?
D1.2 doesn't specify.
Discussion on AWS forum seems to indicate 1/2" beyond all cracks or grind and verify crack is totally removed using dye penetrant or other inspection equipment and techniques.
Anybody here have thoughts? I'm likely going to run an FEA to determine the effects of the HAZ being left in place but I also want input from others.