Good Day!

As per Aws D1.4 2011 Table 6.3 (In-Direct butt) the minimum test specimen is 2. But it requires 2 full section tensile test and 2 macro test.

Is my interpretation correct that the 2 test can be done on each specimen?which part I can use for the macro test?or do I need a total of 4 specimens for each test.

Thanks in advance.

Mike
 