Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AWS welding engineer exam

Status
Not open for further replies.

nabeel3

Mechanical
Dec 14, 2006
145
Hello,

In the syllabus for AWS CWEng exam, two surfacing process are mentioned as SW, THSP. Anyone have idea what it is?
Reference AWS B5. 16
 
Replies continue below

Recommended for you

You will find your answer in AWS A3.0 Standard welding Terms and Definitions. You'll need a copy if you plan on taking the CWEng examination.

Best regards - Al
 
SW - Arc Stud Welding
THSP - Thermal Spray

Best regards - Al
 