B31.3 Restore of thickness/cosmetic repair

Status
Not open for further replies.

WBH

Mechanical
Apr 16, 2003
37
I am looking for code based responses to this question.

Does B31.3 address restoration of thickness of pipe (not weld metal) by addition of weld metal?

Does B31.3 address sharp edges as stress rises, or state that welds shall be free from such?

Are there any limits to restoration after hydrotest has been conducted, to a specific depth?





 
Replies continue below

Recommended for you

WBH;
Do you have a copy of B31.3? If so, please review the following suggestions;

Review 328.6 - this also applies to base metal repairs, as is for weld metal repairs.

Review Table 341.3.2

If ANY weld repairs are required, re-hydrotest. Review 345.2.6.
 