Ben4piping
Mechanical
- Aug 29, 2001
- 15
I have questions pertaining to the metal groups noted in ASME B31.3, Table 304.1.1 Values of Coefficient Y?:
Ferritic steels: Are they only the 400 series SS, duplex, and super duplex austenitic-ferritic SS?
Austenitic stainless steels: Are they 300 series SS and super SS (904L SS)?
Other ductile metals: Are they carbon steels, alloy carbon steels, and non-ferrous metals (Al, Cu, Sn, Ni, Ti, Zr)?
I may have been confusing ferritic with ferrous.
I am aware that increasing the Y value increases allowable pressure.
Thanks, Ben Nottingham
Ferritic steels: Are they only the 400 series SS, duplex, and super duplex austenitic-ferritic SS?
Austenitic stainless steels: Are they 300 series SS and super SS (904L SS)?
Other ductile metals: Are they carbon steels, alloy carbon steels, and non-ferrous metals (Al, Cu, Sn, Ni, Ti, Zr)?
I may have been confusing ferritic with ferrous.
I am aware that increasing the Y value increases allowable pressure.
Thanks, Ben Nottingham